After sanding the body to 220 grit, I filled the grain with some neutral Timber Mate mixed with water. |
I brushed two coats of the soupy mixture over the entire body and allowed two hours of dry time between coats. |
After the Timber Mate had been allowed to fully dry, I sanded off the excess with 220 grit paper. |
Next, I vacuumed off the dust and brushed on a couple of coats of water-based lacquer thinned 1:1 with water. This layer of lacquer will seal the surface and prepare it for the next step. |